Aloyi wa nikeliWaya wowotchereraERNiCr-3
| Miyezo |
| EN ISO 18274 - Ni 6082 - NiCr20Mn3Nb |
| AWS A5.14 – ER NiCr-3 |
Makhalidwe ndi Mapulogalamu
Aloyi 82 imagwiritsidwa ntchito polumikiza ma aloyi 600, 601, 690, 800 ndi 800HT ndi zina zotero.
Chitsulo cholumikizidwa ndi weld chili ndi mphamvu zambiri komanso kukana dzimbiri, kuphatikizapo kukana okosijeni ndi mphamvu yophulika kwa mafunde pa kutentha kwakukulu.
Yabwino kwambiri pakugwiritsa ntchito zowotcherera zosiyanasiyana pakati pa mitundu yosiyanasiyananikelizitsulo zosapanga dzimbiri, zitsulo za kaboni kuphatikizapo zophimba pamwamba.
Yoyenera kugwiritsidwa ntchito kuyambira kutentha kwambiri mpaka kutentha kwambiri, zomwe zimapangitsa kuti alloy iyi ikhale imodzi mwazomwe zimagwiritsidwa ntchito kwambiri.nikelibanja.
Kudula bwino kwa waya kuti ugwiritse ntchito bwino kwambiri.
Kawirikawiri amagwiritsidwa ntchito m'mafakitale opanga magetsi ndi petrochemical etc.
Zipangizo Zachikhalidwe Zoyambira
Aloyi 600, Aloyi 601, Aloyi 690, Aloyi 800, Aloyi 330*
* Mndandanda wofotokozera, osati wodzaza
| Kuphatikizika kwa Mankhwala % | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | |
| kuchuluka | 2.50 | kuchuluka | kuchuluka | kuchuluka | kuchuluka | |
| 0.05 | 3.50 | 3.00 | 0.030 | 0.015 | 0.50 | |
| Cu% | Ni% | Co% | Ti% | Cr% | Nb+Ta% | |
| kuchuluka | 67.00 | kuchuluka | kuchuluka | 18.00 | 2.00 | |
| 0.50 | mphindi | 1.00 | 0.75 | 22.00 | 3.00 | |
| Kulimba kwamakokedwe | ≥600 MPa |
| Mphamvu Yopereka | ≥360 MPa |
| Kutalikitsa | ≥30 MPa |
| Mphamvu Yokhudza Mphamvu | ≥100 MPa |
Kapangidwe ka makina ndi koyerekeza ndipo kamasiyana malinga ndi kutentha, mpweya woteteza, magawo a kuwotcherera ndi zina.
Mpweya Woteteza
EN ISO 14175 – I1, I3
Malo Owotcherera
TS EN ISO 6947 PA, PB, PC, PD, PE, PF
| Deta Yogulira | |||
| M'mimba mwake | Kulemera | Spool | Kuchuluka kwa mphasa |
| 1.00 mm 1.20 mm | Makilogalamu 15 Makilogalamu 15 | BS300 BS300 | 72 72 |
Udindo: Ngakhale kuti pakhala kuyesetsa kotheratu kuti zitsimikizidwe kuti zomwe zili mkati ndi zolondola, izi zitha kusintha popanda kudziwitsa ndipo zitha kuonedwa ngati zoyenera kutsatiridwa ndi anthu onse.