Waya wa Nickel Alloy Welding ERNiCrCoMo-1 Nickel Tig Wire Filler Chitsulo

Kufotokozera Kwachidule:

Aloyi 617 (ERNiCrCoMo-1) ndi waya wotentha kwambiri womwe umagwiritsidwa ntchito powotcherera ma nickel-chromium-cobalt-molybdenum alloys.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Nickel AlloyWaya WowotchereraTig WayaERNiCrCoMo-1

 

Miyezo
EN ISO 18274 - Ni 6617 - NiCr22Co12Mo9
AWS A5.14 - ER NiCrCoMo-1

 

Features ndi Mapulogalamu

Aloyi 617 ndi waya wotentha kwambiri womwe umagwiritsidwa ntchito powotchereranickel- chromium-cobalt-molybdenum aloyi.

Ndibwino kuti muvale zokutira pomwe ma aloyi ofanana amafunikira, monga ma turbine a gasi ndi zida za ethylene.

Oyenera kujowina ma aloyi osiyana komwe mphamvu ya kutentha kwambiri ndi kukana kwa okosijeni zimafunikira mpaka pafupifupi 1150 ° C.

Amagwiritsidwa ntchito muzamlengalenga ndi mafakitale opanga magetsi, kuphatikiza zomera za petrochemical zogwiritsidwa ntchito monga nitric acid chothandizira grids etc.

Zida Zomwe Zimayambira

Ma aloyi a Inconel 600 ndi 601, aloyi a Inkoloy 800 HT ndi 802 ndi ma aloyi opangidwa monga HK40, HP ndi HP45 Modified.Nambala ya UNS N06617, 2.4663, 1.4952, 1.4958, 1.4959, NiCr21Co12Mo, X6CrNiNbN 25 20, X5NiCrAlTi 31 20, X8NiCrAlTi 32 2081, Alloy 32 2081, Alloy
* Mndandanda wazithunzi, osati wokwanira

 

 

Chemical Composition%

C%

Mn%

Fe%

P%

S%

Si%

Ku%

0.05

max

max

max

max

max

max

0.10

1.00

1.00

0.020

0.015

0.50

0.50

Ndi%

Co%

Al%

Ti%

Cr%

Mo%

44.00

10.00

0.80

max

20.00

8.00

min

14.00

1.50

0.60

24.00

10.00

 

Mechanical Properties
Kulimba kwamakokedwe ≥620 MPa
Zokolola Mphamvu -
Elongation -
Mphamvu Zamphamvu -

Makina amakina ndi oyerekeza ndipo amatha kusiyanasiyana kutengera kutentha, kutchingira mpweya, zowotcherera ndi zina.

 

Kuteteza Magesi

TS EN ISO 14175 TIG: I1 (Argon)

 

Malo Owotcherera

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Packaging Data

Diameter

Utali

Kulemera

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

 

Udindo: Ngakhale zoyesayesa zonse zakhala zikuchitika kuti zitsimikizire kulondola kwa zomwe zili, chidziwitsochi chikhoza kusintha popanda chidziwitso ndipo chitha kuonedwa ngati choyenera kuwongolera wamba.