Stainless Steel Welding Electrode AWS A5.4 E2553-16 Ndodo Electrodes yokhala ndi Titanium-Calcium Coating

Kufotokozera Kwachidule:

AF2553-16 (AWS E2553-16) ndi nayitrogeni wokhala ndi duplex zitsulo zosapanga dzimbiri zokhala ndi zokutira za titaniyamu-calcium.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Welding Stainless Steel WeldingElectrode

AF2553-16

GB/T E2553-16

AWS A5.4 E2553-16

Kufotokozera: AF2553-16 ndi electrode yokhala ndi nayitrogeni yokhala ndi duplex chitsulo chosapanga dzimbiri yokhala ndi zokutira za titaniyamu-calcium.Itha kugwiritsidwa ntchito pa AC ndi DC ndikuchita bwino kwambiri.Chifukwa imakhala ndi molybdenum ndi nayitrogeni, komanso mpweya wa kaboni ndi wotsika kwambiri, chitsulo choyikidwacho chimakhala ndi mphamvu yolimbana ndi ming'alu ndi dzimbiri, makamaka kupsinjika kwa dzimbiri.

Ntchito: Amagwiritsidwa ntchito kuwotcherera duplex zitsulo zosapanga dzimbiri zomwe zili ndi chromium pafupifupi 25%, monga 022Cr25Ni7Mo4N, 03Cr25Ni6Mo3Cu2N, UNS 32550 (Alloy255), etc.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Si

Cr

Ni

Mo

Cu

N

S

P

≤0.06

0.5 ~ 1.5

≤1.0

24.0 ~ 27.0

6.5 ~ 8.5

2.9-3.9

1.5 ~ 2.5

0.10 ~ 0.25

≤0.030

≤0.040

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Elongation

%

Zotsimikizika

≥760

≥15

 

Zomwe tikulimbikitsidwa:

Ndodo diameter

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50-80

80-110

110 ~ 160

160 ~ 200

 

Zindikirani:

1. Elekitirodi iyenera kuphikidwa kwa ola limodzi mozungulira 250 ℃ isanayambe ntchito yowotcherera;

2. Gwiritsani ntchito magetsi a DC momwe mungathere, ndipo mphamvuyi isakhale yayikulu kwambiri kuti mupewe kufiira kwa ndodo yowotcherera;

3. Musanayambe kuwotcherera, chotsani mafuta, dzimbiri, sikelo, chinyezi ndi zonyansa zina pamtunda wa mbali zowotcherera.

 

 

Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelectrode kuwotchereras, ndodo zowotcherera,ndikuwotcherera consumableskwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo zitsulo zosapanga dzimbirielectrode kuwotchereras, mpweya zitsulo kuwotcherera maelekitirodi, low aloyi kuwotcherera maelekitirodi, surfacing ma elekitirodi kuwotcherera, faifi tambala & cobalt aloyi kuwotcherera maelekitirodi, wofatsa zitsulo & otsika aloyi mawaya kuwotcherera, zitsulo zosapanga dzimbiri kuwotcherera mawaya, mpweya wotetezedwa flux cored mawaya, aluminium kuwotcherera mawaya, kumizidwa arc kuwotcherera .mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.

 

 


  • Zam'mbuyo:
  • Ena: