Elekitirodi yachitsulo cha kaboni yochepa ya haidrojeni E6011

Kufotokozera Kwachidule:

AWS E6011elekitirodi yowotchererandi mtundu wa cellulose potassium, womwe umagwiritsidwa ntchito powotcherera molunjika. Powotcherera AC ndi DC.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Kugwiritsa ntchito
Ndodo zolumikizira AWS E6011 ndizoyenera kulumikiza zombo monga nyumba ndi milatho, matanki osungiramo zinthu, mapaipi ndi zolumikizira zolumikizira zopondereza.

AWS E6011elekitirodi yowotchereraNdi mtundu wa cellulose potassium, womwe umagwiritsidwa ntchito powotcherera molunjika. Powotcherera AC ndi DC. Umagwiritsa ntchito ukadaulo wapamwamba wakunja ndipo uli ndi luso labwino kwambiri lowotcherera. Kutalika kwa ARC kuyenera kulamulidwa pamlingo woyenera. Sikoyenera kuwotcherera multilayer ndi kuwotcherera cover.

Kapangidwe ka Mankhwala (%)
C Mn Si S P
≤0.2 0.3-0.6 ≤0.22 ≤0.03 ≤0.04
Katundu wa Makina a Chitsulo Chosungidwa
Chinthu Choyesera Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Mtengo Wotsimikizira ≥420 ≥330 ≥22 ≥47
Zotsatira Zonse 485 380 24 86
Ma Reference Current (DC)
M'mimba mwake φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

Mtundu wa Current: Direct Current Electrode Positive (DCEP) kapena AC

NJIRA ZOTHANDIZIRA KUWOTIRA:

Kutalika kwa Arc – Kutalika kwapakati (1/8” mpaka 1/4”)

Lathyathyathya - Khalani patsogolo pa dziwe ndipo gwiritsani ntchito kukwapula pang'ono

Chopingasa - Chopingasa pang'ono cholunjika pamwamba pa mbale

Woyimirira Mmwamba - Njira yokwapula pang'ono kapena yolukira

Woyima Pansi - Gwiritsani ntchito mphamvu yamagetsi yapamwamba komanso kuyenda mwachangu, kukhala patsogolo pa dziwe lamadzi

Pamwamba - Khalani patsogolo pa dziwe ndipo gwiritsani ntchito mayendedwe omenya pang'ono

Chenjezo:
1. N'zosavuta kuziyika pamalo ouma, chonde sungani pamalo ouma.
2. Imafunika kutenthedwa ikasweka phukusi kapena ikalowa chinyezi, kutentha kwa kutentha kuyenera kukhala pakati pa 70C mpaka 80C, nthawi yotenthetsera iyenera kukhala kuyambira 0.5 mpaka ola limodzi.
3. Mukagwiritsa ntchito ma electrode olumikizira magetsi a 5.0mm, ndi bwino kugwiritsa ntchito mphamvu yamagetsi yamphamvu komanso yotsika, kuti muwongolere magwiridwe antchito a magetsi.