Deposited Metal Analysis (Makhalidwe abwino)

C

Mn

Si

Cr

Mo

V

0.5%

0.3%

0.7%

7%

0.5%

0.5%

 

Makhalidwe:

B- 84 ndi electrode yopaka zolimba pazitsulo za alloy ndi carbon steels.Mikanda yokhala ndi malo osalala, yopanda ming'alu ndi pores, imayika zinthu zolimba zomwe zimalimbana ndi abrasion komanso kukhudza kwapakati.Zosavuta kuwotcherera m'malo onse kupatula ofukula pansi.

Katundu Wamakina:Kulimba kuchokera 55 mpaka 60 HRc (za zigawo)

Malo Owotcherera:Yathyathyathya, Yopingasa, Pamwamba, Yoyimirira Mmwamba.

 

Panopa ndi Polarity:

Kwa alternating kapena Direct current

Electrode kupita ku mtengo wabwino

ine mm

ø inu

Amperage

3.20

1/8

100-130

4.00

5/32

120-160

5.00

2/16

180-220

 

Zofunsira: • Zoyenera kukonzanso zida za miyala, kukwera, kubowola

• Laminating masikono

• Makina osindikizira

• Makina oyendetsa dziko lapansi

• Kumeta zipeni.

 

Utali: 350mm.

KULEMERA PA BOKSI: 20 kg / 44 lbs.

 

Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelectrode kuwotchereras, ndodo zowotcherera, ndi kuwotcherera consumables kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo ma elekitirodi osapanga dzimbiri, ma electrodes okotcherera kaboni, maelekitirodi owotcherera a aloyi, ma elekitirodi owotcherera, nickel & cobalt alloy kuwotcherera maelekitirodi, chitsulo chofatsa & otsika mawaya owotcherera, mawaya chitsulo chosapanga dzimbiri, mawaya otetezedwa ndi mpweya, mawaya otetezedwa ndi mpweya, mawaya owotcherera a aluminiyamu, kuwotcherera arc pansi pamadzi.mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.

 

 

 

 


  • Zam'mbuyo:
  • Ena: