D256 (B-80) Electrode Yowotcherera Yolimba, Ndodo Yowotcherera Yokwera, Ndodo ya Arc Welding

Kufotokozera Kwachidule:

Elekitirodi yoyambira yomwe imayika chitsulo cha austenitic manganese, chomwe chimalimba ndi kupindika kozizira, chomwe chimagwiritsidwa ntchito pazitsulo zamtundu womwewo komanso pazigawo zomwe zimakhudzidwa kwambiri ndi kuyanika kwapakatikati.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Electrode Yowotcherera Yowotcherera YolimbaRODO P

RODO PARA RECUBRIMIENTO PROTECTOR

Mtengo wa D256B-80)

Deposited Metal Analysis (Makhalidwe abwino)

C

1.2%

Mn

13.0%

Si

0.5%

Ni

3.0%

 

Makhalidwe:

Elekitirodi yoyambira yomwe imayika chitsulo cha austenitic manganese, chomwe chimalimba ndi kupindika kozizira, chomwe chimagwiritsidwa ntchito pazitsulo zamtundu womwewo komanso pazigawo zomwe zimakhudzidwa kwambiri ndi kuyanika kwapakatikati.Ndizoyenera kuchira, zokutira ndi kukonza zida zachitsulo za austenitic Mn, magawo ndi zidutswa zamakina olemera.

 

Katundu Wamakina:Kuuma 200-250 HB BRINELL pa deposit, 300-400 HB Brinell

pambuyo ozizira ntchito kuumitsa.

 

Malo Owotcherera:Yathyathyathya, Yopingasa, Pamwamba, Yoyimirira Mmwamba.

 

Panopa ndi Polarity:

Kwa alternating kapena Direct current

electrode kukhala positive pole

ine mm

ø inu

Amperage

3.20

1/8

110-130

4.00

5/32

140-160

5.00

2/16

180-230

 

Ntchito: • Kudzaza zitsulo za Manganese.

• Kumanganso mano ndi ndowa zofukula.

• Kuwoloka ndi mitima ya njanji.

• Mphero ndi nyundo.

• Pomenya nyundo kuuma kwake kumawonjezeka kufika ku 350 - 400 HB.

• Mukamamanganso kapena mukukokeranso, gwiritsani ntchito AG AR-91 ngati maziko.

• Pa kutentha pamwamba pa 300 OC, Mn zitsulo

Iwo amayamba kutaya kulimba.Laces akulimbikitsidwa

kulumpha, osachepera awiri ndi amperage zotheka.

 

 

Utali: 350mm.

KULEMERA PA BOKSI: 20 kg / 44 lbs.

 

Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelectrode kuwotchereras, ndodo zowotcherera, ndi kuwotcherera consumables kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zimaphatikizapo zitsulo zosapanga dzimbirielectrode kuwotchereras, mpweya zitsulo kuwotcherera maelekitirodi, low aloyi kuwotcherera maelekitirodi, surfacing ma elekitirodi kuwotcherera, faifi tambala & cobalt aloyi kuwotcherera maelekitirodi, wofatsa zitsulo & otsika aloyi mawaya kuwotcherera, zitsulo zosapanga dzimbiri kuwotcherera mawaya, mpweya wotetezedwa flux cored mawaya, aluminium kuwotcherera mawaya, kumizidwa arc kuwotcherera .mawaya, mawaya a nickel & cobalt alloy kuwotcherera, mawaya owotcherera amkuwa, waya wowotcherera wa TIG & MIG, ma elekitirodi a tungsten, ma elekitirodi a carbon gouging, ndi zida zina zowotcherera & zowonjezera.

 

 

 

 