Kufotokozera Kwachidule:

Elekitirodi yolumikizira ya mtundu wa titaniyamu yachitsulo chosapanga dzimbiri chotsika kwambiri.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Gulu:

AWS A5.4 / ASME SFA5.4 E308-16

JIS Z3221 D308-16

Kufotokozera:

Chitsulo chosapanga dzimbiri chowotcherera maelekitirodiE308-16 ndi mtundu wa titaniyamu wopangidwa ndi mzereelekitirodi yowotchereraChitsulo chosapanga dzimbiri chopanda kaboni wambiri. Chitsulo chosungunula chili ndi mphamvu zabwino kwambiri zamakanika ndipo chimalimbana bwino ndi dzimbiri chifukwa cha kuchuluka kwa kaboni komwe kali mkati mwake ndi ≤. 0.04% b. Chingagwiritsidwe ntchito posungunula malo onse okhala ndi magwiridwe antchito abwino kwambiri: arc yokhazikika, madontho ang'onoang'ono, mawonekedwe abwino a weld. Komansoelekitirodi yowotchereraImakhala ndi mphamvu yolimbana ndi kutentha, siimakhala yofiira mosavuta ndipo mpweya wake suli woboola.

Ntchito:

Kuwotcherera kwa chitsulo cha 18% Cr-8% Ni.

Ndi yoyenera kupangira zolumikizira zopangidwa ndi chitsulo chosapanga dzimbiri cha 022Cr-19Ni10 chotsika kwambiri, monga ulusi wopangira, feteleza,

zida za petrochemical, ndi zina zotero.

Kapangidwe ka Mankhwala a Chitsulo Chosungidwa (E308L-16) (%)

Chinthu C Mn Si Cr Ni S P Cu Mo
mtengo wokhazikika ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
Mtengo wa chitsanzo 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

Katundu wa Makina a Chitsulo Chosungidwa (%)

Mphamvu yolimbana ndi dzimbiri komanso kapangidwe ka ferrite ziyenera kudziwika pakati pa wogula ndi wogulitsa.

Chinthu Mphamvu Yokoka (MPa) Kutalika (%)
mtengo wokhazikika ≥550 ≥25
Mtengo wa chitsanzo 601 41

M'mimba mwake (mm)

2.0

2.5

3.2

4.0

5.0

Kuwotcherera Mphamvu (A)

25-50

50-80

80-110

110-160

160-200

 

Malangizo Okhudza Kugwiritsa Ntchito:

1. Sungani mzere waufupi momwe mungathere.

2. Chotsani dothi monga mafuta ndi fumbi kuchokera mumzere.

3. Umitsani ma electrode pa madigiri 350 (662) kwa mphindi 60 musanagwiritse ntchito