ERNiCrMo-10 imagwiritsidwa ntchito powotcherera zida zoyambira za nickel-chromium-molybdenum kwa iwo okha, zitsulo ndi ma alloys ena a faifi tambala, komanso zomangira zitsulo.Atha kugwiritsidwa ntchito kuwotcherera duplex, super duplex zitsulo zosapanga dzimbiri.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

MAFOTOKOZEDWE AKATUNDU:

AWS: A5.14

Zimagwirizana ndi Chitsimikizo: AWS A5.14 ASME SFA A5.14

Weld Njira: GMAW & ASAW kuwotcherera Njira

ERNiCrMo-10 imagwiritsidwa ntchito powotcherera zida zoyambira za nickel-chromium-molybdenum kwa iwo okha, zitsulo ndi ma alloys ena a faifi tambala, komanso zomangira zitsulo.Atha kugwiritsidwa ntchito kuwotcherera duplex, super duplex zitsulo zosapanga dzimbiri.

Zofunikira za AWS Chemical Composition

C = 0.015 max Ku = 0.50 max
Mn = 1.0 max Ndi = Zotsalira
Fe = 3.0 max Co = 2.0 max
P = 0.04 max Kr = 14.0 - 18.0
S = 0.03 max Mo = 14.0 - 18.0
Si = 0.08 max W = 0.50 max
Zina = 0.50 max Ti = 0.70 max

CHONDE IMBANI KUDZIWA ZAMBIRI NDI MAKULU OPEZA:

Kugwiritsa ntchito

ERNiCrMo-7 imagwiritsidwa ntchito pakuwotcherera zida zoyambira za nickel-chromium-molybdenum yokha, chitsulo ndi ma aloyi ena a faifi tambala komanso kuyika zitsulo ndi NI-CR-MO weld material.

PRODUCT ZITHUNZI:

Kupangidwa Kwakemisiri % (Yodziwika)
C = 0.01 Kr = 16.5 Ndi = Balance
Fe = 2.20 MO = 15.75
Zida Zonse za Weld Metal % (AW)
Kulimba kwamakokedwe 113,00 psi
Elongation 29%

ZINTHU ZOPHUNZITSIDWA ZA CHARPY-V-NOTCH IMPACT:

Zosafunika

Zowotcherera Zomwe Zalimbikitsidwa za MIG ndi SAW Welding ya Nickel Alloys
Njira Diameter of Wire Mphamvu yamagetsi (V) Amperage (A) Gasi
MIG .035 mu 26-29 150-190 75% Argon + 25% Helium
.045 mu 28-32 180-220 75% Argon + 25% Helium
1/16 inchi 29-33 200-250 75% Argon + 25% Helium
SAW 3/32 inchi 28-30 270-350 Flux Yoyenera Itha Kugwiritsidwa Ntchito.
1/8 inchi 29-32 350-450 Flux Yoyenera Itha Kugwiritsidwa Ntchito.
5/32 inchi 30-33 400-550 Flux Yoyenera Itha Kugwiritsidwa Ntchito.