Nickel Alloy Welding Waya ERNiCrMo-10 Tig Waya

Kufotokozera Kwachidule:

Nickel-chromium-molybdenum alloy yopangidwira kujowina C22, 625, 825 kapena kuphatikiza kwa ma aloyi awa.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Nickel AlloyWaya WowotchereraTig WayaERNiCrMo-10

 

 

Miyezo
EN ISO 18274 - Ni 6022 - NiCr21Mo13Fe4W3
AWS A5.14 - ER NiCrMo-10

 

Features ndi Mapulogalamu

Nickel-chromium-molybdenum alloy yopangidwira kujowina C22, 625, 825 kapena kuphatikiza kwa ma aloyi awa.

Amapereka chitsulo cholimba cha Nb-free weld chopangira ma weld osiyanasiyana muzitsulo zosapanga dzimbiri zosapanga dzimbiri za duplex.

Amapereka kukana kwabwino kwambiri polimbana ndi nkhawa & kung'ambika kwa dzimbiri, kukhetsa ndi kuphulika kwa mng'alu.

Amagwiritsidwa ntchito kwambiri pakumangirira ndi kutsekereza zitsulo zotsika za alloy.

Amagwiritsidwa ntchito powotcherera zinthu zowononga kwambiri m'mafakitale opangira mankhwala, zotchingira zolimbana ndi dzimbiri komanso m'malo owopsa am'mphepete mwa nyanja ndi petrochemical etc.

Zikalata Zoyesa zitha kupezeka pa intaneti @wilkinsonstar247.com

Zida Zomwe Zimayambira

Aloyi 22, Aloyi 625, Aloyi 825, Aloyi 926*
* Mndandanda wazithunzi, osati wokwanira

 

 

Chemical Composition%

C%

Mn%

Fe%

P%

S%

Si%

Ku%

max

max

2.00

max

max

max

max

0.010

0.50

6.00

0.020

0.010

0.08

0.50

Ndi%

Co%

Cr%

Mo%

V%

W%

49.00

max

20.00

12.50

max

2.50

min

2.50

22.50

14.50

0.30

3.50

Mechanical Properties
Kulimba kwamakokedwe ≥690 MPa
Zokolola Mphamvu -
Elongation -
Mphamvu Zamphamvu -

Makina amakina ndi oyerekeza ndipo amatha kusiyanasiyana kutengera kutentha, kutchingira mpweya, zowotcherera ndi zina.

 

Kuteteza Magesi

TS EN ISO 14175 TIG: I1 (Argon)

 

Malo Owotcherera

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Packaging Data
Diameter Utali Kulemera
1.60 mm

2.40 mm

3.20 mm1000 mm

1000 mm

1000 mm5 Kg

5 kg

5 kg

 