Waya Wowotcherera wa Nickel Alloy ERNiCu-7 Nickel Tig Wire Filler Chitsulo

Kufotokozera Kwachidule:

ERNiCu-7 ndi aloyi ya nickel-copper yopangidwira kuwotcherera Monel.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Aloyi wa nikeliWaya wowotchereraWaya wa TigERNiCu-7

Miyezo
EN ISO 18274 - Ni 4060 - NiCu30Mn3Ti
AWS A5.14 – ER NiCu-7

 

Makhalidwe ndi Mapulogalamu

Aloyi wa nickel-copper wopangidwira kuwotcherera Monel.

Mawonekedwe abwino a mikanda komanso kukana dzimbiri bwino mu njira zamchere.

Chitsulo chosungunula chimakhala ndi mphamvu yolimbana ndi zinthu zambiri zowononga.

Alloy iyi imagwiritsidwanso ntchito popangira weld.

Kawirikawiri amagwiritsidwa ntchito popanga zinthu za m'madzi, makamaka m'mphepete mwa nyanja, zosinthira kutentha, mapaipi, mafakitale ochotsa mchere m'madzi, mafakitale a mankhwala, petrochemical ndi mphamvu ndi zina zotero.

Zipangizo Zachikhalidwe Zoyambira

Ma aloyi a Monel 400 ndi 404*
* Mndandanda wofotokozera, osati wodzaza

 

 

Kuphatikizika kwa Mankhwala %

C%

Mn%

Fe%

P%

S%

Si%

kuchuluka

3.00

0.50

kuchuluka

kuchuluka

kuchuluka

0.15

4.00

2.50

0.020

0.015

1.00

Cu%

Ni%

Co%

Ti%

Al%

Nb+Ta%

28.00

62.00

kuchuluka

1.50

kuchuluka

kuchuluka

32.00

69.00

1.00

3.00

1.00

0.50

 

Katundu wa Makina
Kulimba kwamakokedwe ≥450 MPa
Mphamvu Yopereka ≥180 MPa
Kutalikitsa ≥30%
Mphamvu Yokhudza Mphamvu ≥80 J

Kapangidwe ka makina ndi koyerekeza ndipo kamasiyana malinga ndi kutentha, mpweya woteteza, magawo a kuwotcherera ndi zina.

 

Mpweya Woteteza

TS EN ISO 14175 TIG: I1 (Argon)

 

Malo Owotcherera

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Deta Yogulira

M'mimba mwake

Utali

Kulemera

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

Makilogalamu 5

Makilogalamu 5

Makilogalamu 5

 

Udindo: Ngakhale kuti pakhala kuyesetsa kotheratu kuti zitsimikizidwe kuti zomwe zili mkati ndi zolondola, izi zitha kusintha popanda kudziwitsa ndipo zitha kuonedwa ngati zoyenera kutsatiridwa ndi anthu onse.