AF2209-15 (AWS E2209-15) Electrode yachitsulo chosapanga dzimbiri yokhala ndi zokutira zochepa za haidrojeni. Ndodo zowotcherera

Kufotokozera Kwachidule:

AF2209-15 (AWS E2209-15) ndi electrode yachitsulo chosapanga dzimbiri yokhala ndi nayitrogeni yochepa kwambiri yokhala ndi hydrogen yochepa.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Kuwotcherera kwa Chitsulo Chosapanga DzimbiriElekitirodi

AF2209-15

GB/T E2209-15

AWS A5.4 E2209-15

Kufotokozera: AF2209-15 ndi electrode yachitsulo chosapanga dzimbiri yokhala ndi nayitrogeni yochepa kwambiri yokhala ndi nayitrogeni yochepa. Gwiritsani ntchito DCEP (electrode yamagetsi yolunjika). Kagwiridwe ka ntchito ndi kabwino kwambiri. Chifukwa ili ndi molybdenum ndi nayitrogeni, ndipo kuchuluka kwa kaboni ndi kochepa kwambiri, chitsulo chomwe chili mu denga chimakhala ndi kukana bwino ming'alu komanso kukana dzimbiri, makamaka kukana dzimbiri.

Kugwiritsa Ntchito: Amagwiritsidwa ntchito makamaka powotcherera zinthu zomwezo zachitsulo chosapanga dzimbiri chotsika kwambiri m'mafakitale amafuta ndi ma hydraulic. Monga kuwotcherera kwa chitsulo chosapanga dzimbiri chopanda 022Cr22Ni5Mo3N.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤0.90

21.5 ~ 23.5

8.5 ~ 10.5

2.5 ~ 3.5

0.08 ~ 0.20

≤0.75

≤0.030

≤0.040

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

Kulimba kwamakokedwe

Mpa

Kutalikitsa

%

Chotsimikizika

≥690

≥20

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

()mm)

2.5

3.2

4.0

5.0

kuwotcherera Current

()A)

50 ~70

80 ~ 110

130 ~ 150

160 ~ 200

 

Zindikirani:

1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha pafupifupi 250℃ isanayambe kuwotcherera;

2. Ndikofunikira kuyeretsa dzimbiri, mafuta oyeretsera, madzi, ndi zinyalala pa zipangizo zowotcherera musanawotchetse.

 

 

Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelekitirodi yowotchereras, ndodo zowotchererandizogwiritsidwa ntchito zowotchererakwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.

 

 