Mpweya Wowotcherera wa Chitsulo cha Carbon
J506Fe13
GB/T E5028
AWS A5.1 E7028
Kufotokozera: J501Fe13 ndi electrode yachitsulo cha kaboni yokhala ndi ufa wachitsulo ndi chofunda chochepa cha hydrogen potaziyamu. AC ndi DC zimagwiritsidwa ntchito kawiri, zoyenera kulumikiza mosabisa komanso kulumikiza mosabisa. Mphamvu yoyikamo ndi pafupifupi 130%.
Kugwiritsa Ntchito: Imagwiritsidwa ntchito powotcherera mopanda chitsulo komanso kuwotcherera mopanda chitsulo cha kaboni ndi chitsulo chotsika cha aloyi, monga Q345, ndi zina zotero.
Kapangidwe ka mankhwala a chitsulo chosungunula (%):
| C | Mn | Si | S | P |
| ≤0.12 | ≤1.60 | ≤0.75 | ≤0.035 | ≤0.035 |
Kapangidwe ka makina a chitsulo chosungunula:
| Chinthu choyesera | Kulimba kwamakokedwe Mpa | Mphamvu yobereka Mpa | Kutalikitsa % | Mtengo wa zotsatira (J) ()-46℃) |
| Chotsimikizika | ≥490 | ≥400 | ≥22 | ≥27 |
Kuchuluka kwa haidrojeni m'chitsulo chosungidwa: ≤8.0mL/100g (njira ya glycerin)
Kuyang'anira X-ray: Giredi II
Mphamvu yovomerezeka:
| M'mimba mwake wa ndodo ()mm) | 4.0 | 5.0 |
| kuwotcherera panopa ()A) | 180 ~ 220 | 210 ~ 260 |
Zindikirani:
1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa 350℃ isanayambe kuwotcherera;
2. Ndikofunikira kuyeretsa dzimbiri, mafuta oyeretsera, madzi, ndi zinyalala pa zipangizo zowotcherera musanawotchetse.
Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zinthu zina zolumikizirana kwa zaka zoposa 20.
Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.