E6010 kaboni chitsulo chowotcherera electrode

Kufotokozera Kwachidule:

E6010 ndi electrode ya rutile-cellulosic sodium.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

AWS E6010 Wofatsa Chitsulo Chowotcherera Electrode

NTCHITO:

Ndi yoyenera kuwotcherera kapangidwe ka chitsulo chotsika mpweya monga mapaipi, zombo ndi mlatho etc.

MAGAWIRIDWE:

AWS A5.1 / ASME SFA5.1 E6010

JIS Z3211 D4310

MAKHALIDWE:

E6010 ndi electrode yamtundu wa rutile-cellulosic sodium. Itha kulumikizidwa kuti igwiritsidwe ntchito bwino (makamaka ngati ili pamalo oyima) ndi DC+ yokha. Ili ndi magwiridwe antchito abwino kwambiri olumikizira monga arc yokhazikika, kudontha pang'ono, kuchotsa slag mosavuta komanso kuthekera kobwezeretsanso zinthu zina. Kuwongolera bwino dziwe losungunuka, mphamvu ya arc yolimba komanso kulowa mozama pamalo oyima.

KUPANGIDWA KWA MANKHWALA A CHITSULO CHONSE: (WOT. %)

Zinthu C Mn Si S P Ni Cr Mo V
Zofunikira ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Zotsatira Zachizolowezi 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

KATUNDU WA MAKANIKO A CHITSULO CHONSE CHOWEDWA:

Zinthu Rm/MPa Rel/Rp0.2 /MPa A/% KV2 (-30℃)/J
Zofunikira ≥430 ≥330 ≥20 ≥27
Zotsatira Zachizolowezi 475 400 26 80

CHENJEZO:

1. Nthawi zambiri, simuyenera kuumitsanso electrode musanayiwotchere. Ngati yakhudzidwa ndi chinyezi, iwumitseninso pa 70℃-90℃ kwa ola limodzi.

2. Dzimbiri, mafuta, madzi ndi zinthu zina zodetsa pamalo opachikira zitsulo ziyenera kuchotsedwa musanapachikire zitsulo.

NJIRA ZOTSATIRA NTCHITO: (DC+)

M'mimba mwake (mm) 2.5 3.2 4.0 5.0
Utali (mm) 300 350 400 400
Mphamvu (A) 50-80 60-100 100-140 140-180

KUPAKA:

5kg/bokosi, mabokosi 4/bokosi, 20kg/bokosi, makatoni 50/mphaleti. 21MT -26MT pa 1X20″ FCL.

 

OEM/ODM:

Timathandizira OEM/ODM ndipo titha kupanga ma CD malinga ndi kapangidwe kanu, chonde titumizireni uthenga kuti tikambirane mwatsatanetsatane.

 

Makhalidwe Ogwiritsira Ntchito:

Mzere wokhazikika kwambiri.

Kuchotsa bwino kwambiri kwa slag.

Kulowa m'malo mwake ndi kosazama.

Kukana kutentha ndi dzimbiri bwino.

Kukana bwino kwambiri ming'alu.


  • Yapitayi: