AWS A5.18 ER70S-6 Carbon Steel Welding Wire Filler Metals for Gas Shielded Arc Welding, Mawaya Olimba

Kufotokozera Kwachidule:

ER70S6 ndi waya wowotcherera wachitsulo wofatsa womwe uli ndi milingo yambiri ya manganese ndi silicon kuposa magiredi ena okhazikika a waya wa MIG kupita ku ma weld apamwamba kwambiri akagwiritsidwa ntchito pazitsulo zakuda, zamafuta, kapena dzimbiri.


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

ER70S6 ndi waya wowotcherera wachitsulo wofatsa womwe uli ndi milingo yambiri ya manganese ndi silicon kuposa magiredi ena okhazikika a waya wa MIG kupita ku ma weld apamwamba kwambiri akagwiritsidwa ntchito pazitsulo zakuda, zamafuta, kapena dzimbiri.Kuchuluka kwa silicon kumawonjezera madzi a dziwe la weld, motero kumapanga mawonekedwe osalala a mikanda ndikupangitsa kuti kugaya pang'ono pambuyo pa weld.Wayayu adapangidwa kuti azipereka ma welds opanda porosity, ma X-ray apamwamba kwambiri (monga momwe amakokedwera) mwa mawaya onse a carbon steel.

Mawonekedwe Ogwiritsa Ntchito: Masitolo anthawi zonse okhala ndi mbale zosakwanira bwino kapena dzimbiri, zamafuta;zitsulo zoponyera zitsulo kapena kupanga salvage;ntchito zapakhomo;pepala lachitsulo;akasinja;ntchito yomanga

Kalasi ya AWS: ER70S6

Chitsimikizo: AWS A5.18/A5.18M:2005

Chingwe: ER70S6

ASME SFA A5.18

Malo Owotcherera: F, V, OH, H

Masiku ano: DCEP

Kuthamanga Kwambiri, kpsi:

70

Kuchuluka kwa Zokolola, kpsi:

58

Kukula mu 2"%:

22

Type Wire Chemistry malinga ndi AWS A5.18 (miyezo imodzi ndiyokwera kwambiri)

C

Mn

Si

P

S

Ni

Cr

Mo

V

Cu

0.06-0.15

1.40-1.85

0.80-1.15

0.025

0.035

0.15

0.15

0.15

0.03

0.50

Zowotcherera Zofananira

Diameter

Njira

Volt

Liwiro Loyenda

Amps

Kuteteza Gasi

in

(mm)

(ipm)

.035

(0.9)

Mtengo wa GMAW

23-26

11-22

160-300

Spray Transfer 98% Argon + 2% Oxygen

.045

(1.2)

Mtengo wa GMAW

23-29

12-21

170-375

Spray Transfer 98% Argon + 2% Oxygen

1/16

(1.6)

Mtengo wa GMAW

25-31

9-19

275-475

Spray Transfer 98% Argon + 2% Oxygen

.023

Mtengo wa GMAW

14-19

10-15

30-85

Kutumiza Kwachidule Kozungulira 98% Argon + 2% Oxygen

.030

(0.8)

Mtengo wa GMAW

15-20

12-24

40-130

Kutumiza Kwachidule Kozungulira 98% Argon + 2% Oxygen

.035

(0.9)

Mtengo wa GMAW

16-25

11-40

60-235

Kutumiza Kwachidule Kozungulira 98% Argon + 2% Oxygen

.045

(1.14)

Mtengo wa GMAW

18-23

12-22

90-290

Kutumiza Kwachidule Kozungulira 98% Argon + 2% Oxygen

.035

(0.9)

Mtengo wa GTAW

12-15

N / A

60-100

100% Argon

.045

(1.14)

Mtengo wa GTAW

13-16

N / A

70-120

100% Argon

1/16

(1.6)

Mtengo wa GTAW

12

N / A

100-160

100% Argon

1/16-3/32

(1.6)-(2.4)

Mtengo wa GTAW

12

N / A

120-250

100% Argon

1/8

(3.2)

Mtengo wa GTAW

12

N / A

150-300

100% Argon