Tyue Brand AWS ENiCrMo-4 Nickel ndi Nickel Based Alloy Welding Electrode, Best Arc Welding Rods, Welding Supplier

Kufotokozera Kwachidule:

Ni327-4 (ENiCrMo-4) ndi electrode yopangidwa ndi nickel yokhala ndi zokutira zochepa za hydrogen sodium.Gwiritsani ntchito DCEP (mwachindunji panopa electrode positive).


Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

Nickel ndi Nickel Alloy Welding Electrode

N327-4                                                     

GB/T ENi6276

AWS A5.11 ENCrMo-4

 

Kufotokozera: Ni327-4 ndi electrode yochokera ku nickel yokhala ndi zokutira zotsika za haidrojeni.Gwiritsani ntchito DCEP (elekitirodi yamakonozabwino).Ili ndi ntchito yabwino kwambiri yowotcherera yokhala ndi kuyaka kokhazikika kwa arc, sipatter yochepa, kuchotsa mosavuta slag,

ndi weld wokongola.The makina katundu wa waikamo zitsulo ndi okhazikika.

 

Ntchito: Ntchito kuwotcherera otsika mpweya faifi tambala-chromium-molybdenum aloyi, monga Hastelloy C276, ASTM B574, B575, B619, B622, B626, ndipo angagwiritsidwe ntchito kuwotcherera zitsulo zosiyana ndi ma aloyi ena faifi tambala.

 

Chemical zikuchokera weld zitsulo (%):

C

Mn

Si

Cr

Ni

Mo

≤0.02

≤1.0

≤0.2

14.5 ~ 16.5

≥50.0

15.0 ~ 17.0

W

Co

Fe

S

P

Zina

3.0 ~ 4.5

≤2.5

4.0 ~ 7.0

≤0.015

≤0.020

≤0.5

 

Zimango za weld zitsulo:

Yesani chinthu

Kulimba kwamakokedwe

Mpa

Zokolola mphamvu

Mpa

Elongation

%

Zotsimikizika

≥690

≥400

≥22

 

Zomwe tikulimbikitsidwa:

Ndodo diameter

(mm)

2.5

3.2

4.0

Welding panopa

(A)

60-90

70 ~ 110

90-150

 

Zindikirani:

1. Elekitirodi iyenera kuphikidwa kwa ola limodzi mozungulira 300 ℃ musanayambe kuwotcherera.Yesani kugwiritsa ntchito arc lalifupi kuti muwotchere;

2. M'pofunika kuyeretsa dzimbiri, mafuta, madzi, ndi zonyansa pazigawo zowotcherera musanayambe kuwotcherera.

3. Yesani kugwiritsa ntchito mphamvu ya mzere waung'ono powotcherera, ma multilayer ndi ma pass-pass kuwotcherera.

 