AWS A5.4 E309-16 Kuweta Chitsulo Chosapanga Chitsulo Chosapanga Chitsulo Choyeretsera Ma Electrode Kuweta Zinthu Zogwiritsidwa Ntchito Zoweta, Ndodo Yowetsera

Kufotokozera Kwachidule:

A302 (AWS E309-16) ndi electrode yachitsulo chosapanga dzimbiri ya Cr23Ni13 yokhala ndi zokutira za titaniyamu-calcium.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Chitsulo chosapanga dzimbiri chowotcherera maelekitirodi

A302                                      

GB/T E309-16

AWS A5.4 E309-16

Kufotokozera: A302 ndi electrode yachitsulo chosapanga dzimbiri ya Cr23Ni13 yokhala ndi zokutira za titaniyamu-calcium. Itha kugwiritsidwa ntchito pa AC ndi DC yokhala ndi magwiridwe antchito abwino kwambiri. Chitsulo chosungidwacho chili ndi kukana kwakukulu kwa ming'alu komanso kukana okosijeni.

Kugwiritsa Ntchito: Amagwiritsidwa ntchito polukira chitsulo chosapanga dzimbiri, chitsulo chosapanga dzimbiri, chitsulo chooneka ngati chapadera (Cr19Ni9 ndi yofanana ndi chitsulo chotsika mpweya), chitsulo cha chromium yambiri, chitsulo cha manganese yambiri, ndi zina zotero.

 

Kapangidwe ka mankhwala a chitsulo chosungunula (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Kapangidwe ka makina a chitsulo chosungunula:

Chinthu choyesera

Kulimba kwamakokedwe

Mpa

Kutalikitsa

%

Chotsimikizika

≥550

≥25

 

Mphamvu yovomerezeka:

M'mimba mwake wa ndodo

(mm)

2.5

3.2

4.0

5.0

kuwotcherera Current

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Zindikirani:

1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa 150℃ isanayambe kuwotcherera;

2. Popeza kuya kwa kulowa kwa magetsi kumakhala kochepa kwambiri panthawi yolumikiza magetsi a AC, magetsi a DC ayenera kugwiritsidwa ntchito momwe angathere kuti alowe kwambiri. Ndipo mphamvu yamagetsi siyenera kukhala yayikulu kwambiri kuti ndodo yolumikizira magetsi isapse.

 

Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zinthu zina zolumikizirana kwa zaka zoposa 20.

Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.