Kuwotcherera kwa Chitsulo Chosapanga DzimbiriElekitirodi
A042
GB/T E309MoL-16
AWS E309MoL-16
Kufotokozera: A042 ndi electrode yachitsulo chosapanga dzimbiri ya Cr23Ni13Mo2 yokhala ndi kaboni yochepa kwambiri yokhala ndi titaniyamu ya calcium. Ingagwiritsidwe ntchito pa AC ndi DC. Chifukwa chowonjezera kuchuluka koyenera kwa molybdenum, kukana ming'alu ndi kukana dzimbiri kwa chitsulo chosungidwacho kumawonjezeka.
Kugwiritsa Ntchito: Pazinthu zomwezo monga zitsulo zosapanga dzimbiri zosapanga dzimbiri zomwe zimakhala ndi mpweya wochepa kwambiri (monga urea synthesis tower lining) ndi zitsulo zosiyana zowotcherera, ndi zina zotero.
Kapangidwe ka mankhwala a chitsulo chosungunula (%):
| C | Mn | Si | Cr | Ni | Mo | Cu | S | P |
| ≤0.04 | 0.5 ~ 2.5 | ≤0.90 | 22.0 ~ 25.0 | 12.0 ~ 14.0 | 2.0 ~ 3.0 | ≤0.75 | ≤0.030 | ≤0.040 |
Kapangidwe ka makina a chitsulo chosungunula:
| Chinthu choyesera | Kulimba kwamakokedwe Mpa | Kutalikitsa % |
| Chotsimikizika | ≥520 | ≥25 |
Mphamvu yovomerezeka:
| M'mimba mwake wa ndodo (mm) | 2.5 | 3.2 | 4.0 | 5.0 |
| kuwotcherera Current (A) | 50 ~ 80 | 80 ~ 110 | 110 ~ 160 | 160 ~ 200 |
Zindikirani:
1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 150℃ isanayambe kuwotcherera;
2. Popeza kuya kwa kulowa kwa magetsi kumakhala kochepa kwambiri panthawi yolumikiza magetsi a AC, magetsi a DC ayenera kugwiritsidwa ntchito momwe angathere kuti alowe kwambiri. Ndipo mphamvu yamagetsi siyenera kukhala yayikulu kwambiri kuti ndodo yolumikizira magetsi isapse;
3. Kukana dzimbiri kwa chitsulo chosungidwa kumatsimikiziridwa ndi mgwirizano wawiri wa kupereka ndi kufuna.
Wenzhou Tianyu Electronic Co., Ltd. idakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopangaelekitirodi yowotchereras, ndodo zowotchererandizogwiritsidwa ntchito zowotchererakwa zaka zoposa 20.
Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.