Chitsulo chosapanga dzimbiri chowotcherera maelekitirodi
A102
GB/T E308-16
AWS E308-16
Kufotokozera: A102 ndi electrode yachitsulo chosapanga dzimbiri ya Cr19Ni10 yopanda kaboni yokhala ndi titaniyamu-calcium. Itha kugwiritsidwa ntchito pa AC ndi DC ndipo imagwira ntchito bwino. Chitsulo chosungidwacho chili ndi mphamvu zabwino zamakaniko komanso chimalimbana ndi dzimbiri la pakati pa tinthu tating'onoting'ono.
Kugwiritsa Ntchito: Imagwiritsidwa ntchito pa nyumba zosapanga dzimbiri za 06Cr19Ni10 ndi 06Cr18Ni11Ti zomwe sizingawonongeke ndi dzimbiri komanso kutentha kogwiritsa ntchito kulumikiza kosakwana 300°C.
Kapangidwe ka mankhwala a chitsulo chosungunula (%):
| C | Mn | Si | Cr | Ni | Mo | Cu | S | P |
| ≤0.08 | 0.5 ~ 2.5 | ≤0.90 | 18.0 ~ 21.0 | 9.0 ~ 11.0 | ≤0.75 | ≤0.75 | ≤0.030 | ≤0.040 |
Kapangidwe ka makina a chitsulo chosungunula:
| Chinthu choyesera | Kulimba kwamakokedwe Mpa | Kutalikitsa % |
| Chotsimikizika | ≥550 | ≥35 |
Mphamvu yovomerezeka:
| M'mimba mwake wa ndodo (mm) | 2.0 | 2.5 | 3.2 | 4.0 | 5.0 |
| kuwotcherera Current (A) | 25 ~ 50 | 50 ~ 80 | 80 ~ 110 | 110 ~ 160 | 160 ~ 200 |
Zindikirani:
1. Electrode iyenera kuphikidwa kwa ola limodzi pa kutentha kwa pafupifupi 150℃ isanayambe kuwotcherera;
2. Popeza kuya kwa kulowa kwa magetsi kumakhala kochepa kwambiri panthawi yolumikiza magetsi a AC, magetsi a DC ayenera kugwiritsidwa ntchito momwe angathere kuti alowe kwambiri. Ndipo mphamvu yamagetsi siyenera kukhala yayikulu kwambiri kuti ndodo yolumikizira magetsi isapse;
3. Kukana dzimbiri ndi kuchuluka kwa ferrite mu chitsulo chosungidwacho zimatsimikiziridwa ndi mgwirizano wawiri wa kupereka ndi kufunikira.
Kampani ya Wenzhou Tianyu Electronic Co., Ltd. inakhazikitsidwa mu 2000. Takhala tikugwira ntchito yopanga ma electrode olumikizirana, ndodo zolumikizirana, ndi zinthu zina zolumikizirana kwa zaka zoposa 20.
Zogulitsa zathu zazikulu zikuphatikizapo ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo za kaboni, ma electrode olumikizira zitsulo zosapanga dzimbiri, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika, ma electrode olumikizira zitsulo zopindika ndi nickel & cobalt, mawaya olumikizira zitsulo zosapanga dzimbiri & low alloy, mawaya olumikizira zitsulo zosapanga dzimbiri, mawaya olumikizidwa ndi mpweya, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika, mawaya olumikizira zitsulo zopindika ndi nickel & cobalt ... ndi mkuwa, mawaya olumikizira zitsulo zopindika ndi TIG & MIG, ma electrode a tungsten, ma electrode olumikizira zitsulo zopindika ndi kaboni, ndi zina zowonjezera ndi zogwiritsidwa ntchito.